Few questions.
Hello I still new to this and second guessing myself.
First question what is min temperature I should do load development on.
Next is does this look okay to you it's a 308 168 accubond lr I loaded for ar 10 its 2.800. Using win large primers and bl-c2 powder which I'm told can be different with temperature. https://uploads.tapatalk-cdn.com/201...7e00cff838.jpg
Sent from my SM-G960U using Tapatalk
-
Looks fine to me. Any temperature is fine to test loads in. I personally test loads in 50 degree or warmer weather, I don’t shoot as well when I’m miserable. Blc2 is a temp sensitive powder, what is safe in the cold weather, may be high pressure in hot weather, you just need to test it out. I have an armalite ar10 .308. All of my COAL’s are between 2.780 and 2.800, and function fine.
JTD